Creep-Fatigue Life and Cyclic Constitutive Relation of Mar-M247LC Nickel-Base Directionally Solidified Superalloy.

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

Fatigue-creep-environment Interactions in a Directionally-solidified Ni-base Superalloy

Directionally-solidified (DS) GTD-111 is a Ni-base superalloy designed to withstand damage occurring in the first and second stage blades of gas-powered turbines. Because of the distinctive microstructure of this material, the manner in which fatiguecreep-environment damage mechanisms interact to initiate cracks is sensitive to grain structure and chemical composition. Along with fatigue cyclin...

متن کامل

Simulation of Creep Crack Growth of a Directionally-solidified Ni-base Superalloy

Creep lifetime of turbine blade material subjected to sustained centrifugal forces at elevated temperatures is limited by accumulated inelastic deformation and creep crack growth (CCG). Creep resistance exhibited in conventionally cast polycrystalline (PC) Ni-base superalloy components has been enhanced via solidification techniques. Directional solidification (DS) results in large grain sizes ...

متن کامل

Modeling the Temperature-dependence of Tertiary Creep Damage of a Directionally Solidified Ni-base Superalloy

Directionally solidified (DS) Ni-base superalloys have become a commonly used material in gas turbine components. Controlled solidification during the material manufacturing process leads to a special alignment of the grain boundaries within the material. This alignment results in different material properties dependent on the orientation of the material. When used in gas turbine applications t...

متن کامل

Very High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4

The effect of casting pores on the very high cycle fatigue (VHCF) behavior of a directionally solidified (DS) Ni-base superalloy DZ4 is investigated. Casting and hot isostatic pressing (HIP) specimens were subjected to very high cycle fatigue loading in an ambient atmosphere. The results demonstrated that the continuously descending S-N curves were exhibited for both the casting and HIP specime...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1993

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.42.868