Corrosion and Oxidation Behavior of a Fe-Al-Mn-C Duplex Alloy

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Deformation-Induced Defects on the Microstructure and Pitting Corrosion Behavior of Al-Ag Alloy

In this study, a wide range of combined ageing treatments and cold work deformations in the Al 4.2 wt% Ag alloy matrix were proposed, aiming to investigate the effect of defects such as precipitates (Ag2Al plates) and dislocations on the mechanical and electrochemical behavior of Al–4.2 wt% Ag alloys. Further reductions of thickness from 10 to 60%, decreases the mean size of Ag2...

متن کامل

Effect of heterogeneously distributed pre-existing dispersoids on the recrystallization behavior of a cold-rolled Al-Mn-Fe-Si alloy

a r t i c l e i n f o It is well known that strong concurrent precipitation, mainly located along grain/subgrain boundaries, results in a coarse and elongated grain structure, and unusual sharp P {011} b566N and/or M {113} b110N texture components during annealing of supersaturated AA3xxx-series alloys. In this study, a supersaturated as-cast Al–Mn– Fe–Si alloy was annealed at three temperature...

متن کامل

Catalytic oxidation of toluene over LaBO3 (B= Fe, Mn and Co) and LaCo0.7B′0.3O3 (B′= Fe and Mn) perovskite-type

In this paper, LaBO3 perovskite type catalyst formulations were prepared by sol-gel auto combustion method using citric acid as the fuel. Activity of catalysts was tested in catalytic oxidation of toluene as a model of volatile organic compounds. LaCoO3 perovskite formulation showed the highest activity among LaBO3 (Fe, Mn and Co) perovskite catalysts. So, LaCoO3 perovskite based catalyst was s...

متن کامل

Kinetics of Austenite Recrystallization during the Annealing of Cold-rolled Fe-Mn-Al-C Steel

In the current study, the recrystallization behavior of 75% cold-rolled Fe-22Mn-10Al-1.4C steel during annealing at 750, 770, 790, 810, and 830°C was studied. X-ray diffraction patterns and optical microscopy were used to characterize microstructures. The Vickers Micro-hardness test was used to characterize recrystallization kinetics during annealing. Johnson-Mehl-Avrami-Kolmogorov (JMAK) model...

متن کامل

Description to Fe-C Alloy Film Fiber Corrosion Sensors by Fractal Corrosion Images

In this paper, the fractal dimensions are proposed for characterizing the optical fiber corrosion sensors, which is applied to measure the steel corrosion based on Fe-C alloy film. Because corrosion was a complex random phenomenon and the corrosion surface of Fe-C alloy film of the optical fiber corrosion sensor possessed fractal characteristics, the image fractal dimensions is as a quantitativ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials

سال: 2019

ISSN: 1996-1944

DOI: 10.3390/ma12162572