Correlation of rolling condition, microstructure, and low-temperature toughness of X70 pipeline steels

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The effects of chemical composition variations on microstructure and mechanical properties of nanostructured, low temperature bainitic steels

Bainitic transformation at low transformation temperatures leads to a microstructure involving fine plates of bainitic ferrite and thin films of retained austenite. This microstructure has shown ultimate tensile strength of about 2.2 GPa, noticeable uniform elongation in the range of 5 to 30%, hardness values of about 600 to 670 HV and impact toughness in the range of 30 to 40 MPa m1/2. With ca...

متن کامل

Microstructure Evolution of HSLA Pipeline Steels after Hot Uniaxial Compression

The mechanical properties of the high-strength low-alloy pipeline steels were mainly controlled by the subsequent phase transformations after rolling. The influence of hot uniaxial compression on the phase transformation of acicular ferrite was explored by viewing of the deformation degree, the deformation temperature, and the strain rate. The results show that the increase of deformation amoun...

متن کامل

Effect or Inoculation on Microstructure and Properties of Low C-Mn and Low Alloy Steels

Effect of the addition of various inoculants on the morphology and mechanical properties of low C-Mn and low alloy steel samples is studied by thermal and mechanical processing of the samples after solidification. According to the results obtained from metallographic studies with the electron microscope and microanalysis with x-rays, the distribution of inoculating agents in the steel matrix is...

متن کامل

EFFECT OF FINISH ROLLING TEMPERATURE ON MICROSTRUCTURE,TEXTURE AND PLANAR ANISOTROPY IN ALUMINUM ALLOY AA3004 SHEETS

AA3004 alloy is widely used in can making. The major concern in the production of canbodies is earing, which develop by high planar anisotropy of rolled sheet. Balance ofrecrystallisation and rolling textures together with a uniform and fine grain microstructure canminimize the earing. The effects of finish rolling temperature (FRT) on planar anisotropy,microstructure, texture development and m...

متن کامل

the effects of chemical composition variations on microstructure and mechanical properties of nanostructured, low temperature bainitic steels

bainitic transformation at low transformation temperatures leads to a microstructure involving fine plates of bainitic ferrite and thin films of retained austenite. this microstructure has shown ultimate tensile strength of about 2.2 gpa, noticeable uniform elongation in the range of 5 to 30%, hardness values of about 600 to 670 hv and impact toughness in the range of 30 to 40 mpa m1/2. with ca...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions A

سال: 2005

ISSN: 1073-5623,1543-1940

DOI: 10.1007/s11661-005-0043-1