Fast charging of lithium-ion (Li-ion) batteries makes it susceptible to lithium plating. In this study, we report the correlation between capacity loss and cell impedance changes in battery due electrodeposition. Li-ion pouch cells with nickel-manganese-cobalt cathode graphite anode were charged at rates varying from 0.5C 6C. The voltage evolution immediately after was monitored identify C-rates that result Electrochemical spectroscopy (EIS) used monitor evolution. lower than 1C no plating showed minimal their baseline values period charging. However, undergoing higher 3C a substantial reduction charging, recovery back 30 min relaxation. These observations suggest causes damage solid electrolyte interface (SEI) layer on particles during period, followed by reformation SEI relaxation period. measured has linear observed change. relationship suggests monitoring may be for prognostication state-of-health batteries.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Analysis of capacity fade in a lithium ion battery

Two parameter estimation methods are presented for online determination of parameter values using a simple charge/discharge model of a Sony 18650 lithium ion battery. Loss of capacity and resistance increase are both included in the model. The first method is a hybrid combination of batch data reconciliation and moving-horizon parameter estimation. A discussion on the selection of tuning parame...

متن کامل

The role of mechanically induced separator creep in lithium-ion battery capacity fade

Lithium-ion batteries are well-known to be plagued by a gradual loss of capacity and power which occur regardless of use and can be limiting factors in the development of emerging energy technologies. Here we show that separator deformation in response to mechanical stimuli that arise under normal operation and storage conditions, such as external stresses on the battery stack or electrode expa...

متن کامل

Online Diagnosis for the Capacity Fade Fault of a Parallel-Connected Lithium Ion Battery Group

Hua Zhang 1,2, Lei Pei 1, Jinlei Sun 1, Kai Song 1, Rengui Lu 1, Yongping Zhao 1, Chunbo Zhu 1,* and Tiansi Wang 1 1 School of Electrical Engineering and Automation, Harbin Institute of Technology, Harbin 150001, China; [email protected] (H.Z.); [email protected] (L.P.); [email protected] (J.S.); [email protected] (K.S.); [email protected] (R.L.); [email protected] (Y.Z.); tiansi.wa...

متن کامل

Capacity fade analysis of a lithium ion cell

A physics-based single particle model was used to simulate the life cycling data of a lithium ion cell. The simulation indicates that there are robably three stages of capacity fade in a lithium ion cell used at low rates. In the first stage, lithium ions are lost to a film formation reaction (e.g. EI formation) and, consequently, the cathode becomes less intercalated during cycling. In the sec...

متن کامل

A comparison of lead-acid and lithium-based battery behavior and capacity fade in off-grid renewable charging applications

The effects of variable charging rates and incomplete charging in off-grid renewable energy applications are studied by comparing battery degradation rates and mechanisms in lead-acid, LCO (lithium cobalt oxide), LCO-NMC (LCO-lithium nickel manganese cobalt oxide composite), and LFP (lithium iron phosphate) cells charged with wind-based charging protocols. Poor pulse charge acceptance, particul...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Power Sources

سال: 2021

ISSN: ['1873-2755', '0378-7753']

DOI: https://doi.org/10.1016/j.jpowsour.2020.229360