Brittle Fracture Failure of Composite (Non- Ceramic) Insulators

In this work, additional input is provided into the ongoing discussion on the mechanisms, causes and remedies of brittle fracture failures of composite (non-ceramic) insulators. This has been done partially to complement the recently published article on this topic entitled “ IEEE Task Force Report: Brittle Fracture in Non-Ceramic Insulators” [1]. At first, the most important characteristics of...

متن کامل

On an Eigendeformation Approach to Brittle Fracture

The paper presents a numerical implementation of a novel approximation scheme for Griffith’s theory of brittle fracture recently proposed in [1]. The total potential energy of a brittle body (including bulk and surface terms) is variationally approximated by a family of functionals, depending on a small penalty parameter ε. The (two-field) approximating functionals have as arguments the displac...

متن کامل

Fractal Dimension of Brittle Fracture

Using a worldwide catalog of earthquakes we analyze the distribution of distances between pairs of earthquake hypocenters to determine the spatial fractal dimension 6 of an earthquake fracture. As the time span of the catalog increases, 8 asymptotically reaches the value 2.1-2.2 for shallow earthquakes. Approximately the same asymptotic value of dimension is obtained for a catalog of earthquake...

متن کامل

An eigenerosion approach to brittle fracture

The present work is concerned with the verification and validation of a variant of the eigenfracture scheme of Schmidt et al. (2009) based on element erosion, which we refer to as eigenerosion. Eigenerosion is derived from the general eigenfracture scheme by restricting the eigendeformations in a binary sense: they can be either zero, in which case the local behavior is elastic, or they can be ...

متن کامل

Brittle Fracture of 2D MoSe2.

An in situ quantitative tensile testing platform is developed to enable the uniform in-plane loading of a freestanding membrane of 2D materials inside a scanning electron microscope. The in situ tensile testing reveals the brittle fracture of large-area MoSe2 crystals and measures their fracture strength for the first time.

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Strength of Materials

سال: 2020

ISSN: 0039-2316,1573-9325

DOI: 10.1007/s11223-020-00183-w