Warm Pre-Strain: Strengthening the Metastable 304L Austenitic Stainless Steel without Compromising Its Hydrogen Embrittlement Resistance
Plastic pre-strains were applied to the metastable 304L austenitic stainless steel at both room temperature (20 °C) and higher temperatures (i.e., 50, 80 and 100 °C), and then the hydrogen embrittlement (HE) susceptibility of the steel was evaluated by cathodically hydrogen-charging and tensile testing. The 20 °C pre-strain greatly strengthened the steel, but simultaneously significantly increa...
متن کاملOn the Constitutive Model of Nitrogen-Containing Austenitic Stainless Steel 316LN at Elevated Temperature
The nitrogen-containing austenitic stainless steel 316LN has been chosen as the material for nuclear main-pipe, which is one of the key parts in 3rd generation nuclear power plants. In this research, a constitutive model of nitrogen-containing austenitic stainless steel is developed. The true stress-true strain curves obtained from isothermal hot compression tests over a wide range of temperatu...
متن کاملMartensite ? austenite phase transformation kinetics in an ultrafine-grained metastable austenitic stainless steel
A generalized phase transformation kinetics model is used to understand the martensite to austenite transformation in a cold-rolled and annealed metastable AISI 301LN ultrafine-grained austenitic stainless steel. The model shows that the presence of interstitial nitrogen and heavy cold-rolling is important to promote fast transformation kinetics, through rapid nitrogen-diffusion and austenite n...
متن کاملDelayed Cracking of Metastable Austenitic Stainless Steels after Deep Drawing
In metastable austenitic stainless steels, strain-induced martensitic transformation during plastic deformation enhances work hardening of the material, increasing its strength and in some cases also ductility.1,2) The presence of α’-martensite, however, may increase the susceptibility of these materials to hydrogen embrittlement phenomena, for example delayed cracking.3–6) Delayed cracking can...
متن کاملSensitization Behavior of Gnaw Austenitic Stainless Steel Joints
The present work has been carried out to study the sensitization behavior of AISI 304L austenitic stainless steel weld, fabricated using GTAW (gas tungsten arc welding process). This weld was subjected to post weld thermal aging (PWTA) treatments lying in the sensitization range, viz. 700 ?C for 30 minutes, 500 minutes and 1000 minutes for studying the influence of carbide precipitation on thei...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: International Journal of Material Forming
سال: 2008
ISSN: 1960-6206,1960-6214
DOI: 10.1007/s12289-008-0037-9