Pitting Resistance of Pure Fe-17%Cr Alloys: Consequences for Localized Corrosion Modeling

Pitting corrosion was observed on a high purity Fe-17Cr alloy in 0.02M NaCl solution of pH 6.6 at high anodic potential (+ 550 mVISCE). Potentiostatic electrochemical noise measurements were performed, revealing the presence of a characteristic current noise below stable pitting, differing strongly from that observed 011 a series of AISI 430 type 17% Cr stainless steels, with respect to the fre...

متن کامل

Numerical Simulation of Material Strength Deterioration due to Pitting Corrosion

Pitting corrosion is an insidious form of localized corrosion a ecting characteristics of various engineering metallic alloys. Currently very limited literature exists with regard to systematic characterization of pitted surfaces or the efficient use of numerical methods to assess its effect, i.e. fatigue life reduction caused by the state of a corroded specimen and particularly through the stu...

متن کامل

Intergranular pitting corrosion of CoCrMo biomedical implant alloy.

CoCrMo samples of varying microstructure and carbon content were electrochemically corroded in vitro and examined by scanning electron microscopy and electron backscatter diffraction techniques. The rate of corrosion was minimized (80% reduction from icorr = 1396 nA/cm(2) to icorr = 276 nA/cm(2) ) in high-carbon CoCrMo alloys which displayed a coarser grain structure and partially dissolved sec...

متن کامل

Probabilistic Pitting Corrosion Risk Assessment of Welded Offshore Steel Pipelines

Steel structures continuously exposed to offshore marine environments are prone to corrosion. This can be of major economic and perhaps of environmental significance. The risk of these scenarios occurring can be assessed using good quality data, good quality corrosion and pitting models and structural reliability assessment. Recently, improved models for the prediction of longer term corrosion ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Corrosion Reviews

سال: 2019

ISSN: 2191-0316,0334-6005

DOI: 10.1515/corrrev-2019-0049