Comparison Between Stainless Steels and Nickel Alloys Through Pitting Corrosion Resistance Electrochemical Tests
نویسندگان
چکیده
منابع مشابه
Atomic-scale decoration for improving the pitting corrosion resistance of austenitic stainless steels
Stainless steels are susceptible to the localized pitting corrosion that leads to a huge loss to our society. Studies in the past decades confirmed that the pitting events generally originate from the local dissolution in MnS inclusions which are more or less ubiquitous in stainless steels. Although a recent study indicated that endogenous MnCr2O4 nano-octahedra within the MnS medium give rise ...
متن کاملCytotoxicity study of plasma-sprayed hydroxyapatite coating on high nitrogen austenitic stainless steels.
Stainless steel has been frequently used for temporary implants but its use as permanent implants is restricted due to its low pitting corrosion resistance. Nitrogen additions to these steels improve both mechanical properties and corrosion resistance, particularly the pitting and crevice corrosion resistance. Many reports concerning allergic reactions caused by nickel led to the development of...
متن کاملNICKEL RELEASE FROM 304 AND 316 STAINLESS STEELS lN SYNTHETIC SWEAT. COMPARISON WITH NICKEL AND NICKEL-PLA TED MET ALS. CONSEQUENCES ON ALLERGIC CONTACT DERMATITIS
Release of nickel from nickel or nickel-plated metals, is often responsible for allergic contact dermatitis. However, the effect of nickel-bearing stainless steels is not weil known. ln this paper AISI 304, 316 and 430 type stainless steels, as weil as nickel and nickel-plated materials, are investigated. Three tests were carried out: electrochemical tests and leaching experiments in sodium chl...
متن کاملIn Vitro Electrochemical Corrosion and Cell Viability Studies on Nickel-Free Stainless Steel Orthopedic Implants
The corrosion and cell viability behaviors of nanostructured, nickel-free stainless steel implants were studied and compared with AISI 316L. The electrochemical studies were conducted by potentiodynamic polarization and electrochemical impedance spectroscopic measurements in a simulated body fluid. Cytocompatibility was also evaluated by the adhesion behavior of adult human stem cells on the su...
متن کاملEffects of Nitrogen and Tensile Direction on Stress Corrosion Cracking Susceptibility of Ni-Free FeCrMnC-Based Duplex Stainless Steels
Stress corrosion cracking (SCC) behavior of Ni-free duplex stainless steels containing N and C (Febalance-19Cr-8Mn-0.25C-(0.03, 0.21)N, in wt %) was investigated by using a slow strain rate test (SSRT) in air and aqueous NaCl solution with different tensile directions, including parallel (longitudinal) and perpendicular (transverse) to the rolling direction. It was found that alloying N was eff...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Research
سال: 2021
ISSN: 1980-5373,1516-1439
DOI: 10.1590/1980-5373-mr-2020-0386