Colloidal AgSbSe2 nanocrystals: surface analysis, electronic doping and processing into thermoelectric nanomaterials

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electronic Impurity Doping of Colloidal Semiconductor Nanocrystals

Doping is extremely important for controlling the electronic conductivity of bulk semiconductors. However, very few examples exist where impurities that have been incorporated into colloidal semiconductor nanocrystals affect their electronic properties. Here we will discuss the challenges in this area as well as recent progress. In particular, we will describe an approach to lightly dope semico...

متن کامل

Photochemical electronic doping of colloidal CdSe nanocrystals.

A method for electronic doping of colloidal CdSe nanocrystals (NCs) is reported. Anaerobic photoexcitation of CdSe NCs in the presence of a borohydride hole quencher, Li[Et3BH], yields colloidal n-type CdSe NCs possessing extra conduction-band electrons compensated by cations deposited by the hydride hole quencher. The photodoped NCs possess excellent optical quality and display the key spectro...

متن کامل

ChlorineEnabled Electron Doping in SolutionSynthesized SnSe Thermoelectric Nanomaterials

DOI: 10.1002/aenm.201602328 precursors,[4] doping proves challenging for solution-synthesized MC nanostructures.[5] Recently, post-synthesis halide treatment of nanocrystals in solution has been developed which involves switching halogens for long chain surfactant molecules absorbed on the surface.[2,6] In fact, sorption of halogens can be realized as part of a one-pot synthesis using metal hal...

متن کامل

Colloidal Synthesis and Thermoelectric Properties of CuFeSe2 Nanocrystals

Copper-based chalcogenides that contain abundant, low-cost and environmentally-friendly elements, are excellent materials for numerous energy conversion applications, such as photocatalysis, photovoltaics, photoelectricity and thermoelectrics (TE). Here, we present a high-yield and upscalable colloidal synthesis route for the production of monodisperse ternary I-III-VI₂ chalcogenides nanocrysta...

متن کامل

Hypervalent surface interactions for colloidal stability and doping of silicon nanocrystals

Colloidal semiconductor nanocrystals have attracted attention for cost-effective, solution-based deposition of quantum-confined thin films for optoelectronics. However, two significant challenges must be addressed before practical nanocrystal-based devices can be realized. The first is coping with the ligands that terminate the nanocrystal surfaces. Though ligands provide the colloidal stabilit...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Materials Chemistry C

سال: 2016

ISSN: 2050-7526,2050-7534

DOI: 10.1039/c6tc00893c