Chip Formation and Machinability of Nickel-Base Superalloys

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Review on Thermo-Mechanical Fatigue Behavior of Nickel-Base Superalloys

Nickel-base superalloys have become the key materials of hot-end components in the aeroengines over the past several decades. Nickelbase superalloys are easy to produce thermo-mechanical fatigue (TMF) behavior when withstanding the combined effects of high temperature, creep, oxidation, mechanical stress and thermal stress. The occurrence of TMF seriously affects the normal service for hot-end ...

متن کامل

Residual Stress Assessment in Surface-treated Nickel-base Superalloys

Experimental results are presented to illustrate that there exists a unique window of opportunity for eddy current NDE of residual stress in surface-treated nickel-base superalloys. In light of its frequency-dependent penetration depth, the measurement of eddy current conductivity has been suggested as a possible means to allow the nondestructive evaluation of subsurface residual stresses in su...

متن کامل

Strain induced abnormal grain growth in nickel base superalloys

Under certain circumstances abnormal grain growth occurs in Nickel base superalloys during thermomechanical forming. Second phase particles are involved in the phenomenon, since they obviously do not hinder the motion of some boundaries, but the key parameter is here the stored energy difference between adjacent grains. It induces an additional driving force for grain boundary migration that ma...

متن کامل

Recrystallisation of Practical Mechanically Alloyed Iron–Base and and Nickel–Base Superalloys

Commercialised mechanically alloyed yttria dispersion strengthened alloys exhibit unusual recrystallisation behaviour. In spite of their large stored energy content, they tend to recrystallise at temperatures close to melting. The recrystallised microstructure is often very coarse and highly anisotropic, characterised by columnar grains. Such a microstructure is often referred to as being “dire...

متن کامل

Survey and Study of Machinability for Titanium Alloy Ti-6Al-4V through Chip Formation in Milling Process

Most of the materials used in the industry of aero-engine components generally consist of titanium alloys. Advanced materials, because of their excellent combination of high specific strength, light weight and general corrosion resistance. In fact, chemical wear resistance of aero-engine alloy provides a serious challenge for cutting tool material during the machining process. The reduction in ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Advanced Materials Research

سال: 2011

ISSN: 1662-8985

DOI: 10.4028/www.scientific.net/amr.278.460