Characterization on stress-strain behavior of ferrite and austenite in a 2205 duplex stainless steel based on nanoindentation and finite element method

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Study on Static Recrystallization Process in Duplex Stainless Steel 2205

Steel 2205 is one of the most famous duplex stainless steels. The microstructure of this steel composed of ferrite and austenite in similar amount. Therefore, in order to improve mechanical properties through microstructure, thermo mechanical processes such as controlled hot rolling and forging should be applied. It is not possible to employ the usual heat treatment. It shows the importance of ...

متن کامل

Ferrite and austenite phase identification in duplex stainless steel using SPM techniques

It can be challenging to properly identify the phases in electro-polished duplex stainless steel using optical microscopy or other characterization techniques. This letter describes magnetic force microscopy to properly identify the phases in electropolished duplex stainless steel. The results are also confirmed PM anoindentation with the current sensing atomic force and scanning Kelvin probe f...

متن کامل

The Influence of Heat-Input on Structural and Mechanical Properties of 2205 Duplex Stainless Steel

The influence of heat-input and pre-heat treatment on the structure, mechanical and corrosion behaviors of 2205 duplex stainless steel joint by means of GMAW process was the goal of this study. In this regards, the welding process was done using different heat input in the range of 0.6 to 1.4 kJ/mm and different pre-heating treatments in the range of 25 to 100 oC. The microstructural properties...

متن کامل

The Influence of Heat-Input on Structural and Mechanical Properties of 2205 Duplex Stainless Steel

The influence of heat-input and pre-heat treatment on the structure, mechanical and corrosion behaviors of 2205 duplex stainless steel joint by means of GMAW process was the goal of this study. In this regards, the welding process was done using different heat input in the range of 0.6 to 1.4 kJ/mm and different pre-heating treatments in the range of 25 to 100 oC. The microstructural properties...

متن کامل

Crystallography of Widmanstätten austenite in duplex stainless steel weld metal

Two kinds of austenite grow from d-ferrite during the cooling of the duplex stainless steel weld deposits studied here, Widmanstätten plates and allotriomorphs which precipitate at d–d grain boundaries. It is found using microtexture measurements that the preferred crystallographic orientation of the Widmanstätten austenite can be estimated using established theory if it is assumed that there i...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Results in Physics

سال: 2018

ISSN: 2211-3797

DOI: 10.1016/j.rinp.2018.06.023