Characterization of Polymer Fracture by Ultrasonic Fractography.

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Ability of Ultrasonic Characterization to Extract the Dose Distribution of MAGIC-f Polymer Gel

Background & Aims: Today, different imaging techniques have been studied in the reading of radiationsensitive polymer gels dosage. Due to limitations of imaging techniques such as magnetic resonance imaging (MRI) and computed tomography (CT), ultrasound techniques are proposed for dose-dependent parameter extraction. In this study, using MAGIC-f (methacrylic and ascorbic acid in gelatin initiat...

متن کامل

Fractography of Polymer Composites: Current Status and Future Issues

With the increasing prevalence of polymer composites in engineering applications, invariably mechanical failures of these components are occurring. Key to addressing this is fractographic analysis; the examination of fracture surfaces to deduce information about the damage and failure of components. The fractography of isotropic materials, particularly metals, has been used as a tool for many y...

متن کامل

Fractography: fracture topography as a tool in fracture mechanics and stress analysis. An introduction

service Email alerting article to receive free email alerts when new articles cite this click here

متن کامل

Mechanical Characterization and Fractography of Pc, Abs and Pmma – a Comparison of Tensile, Impact and Esc Fracture Surfaces

This work presents an effort to document and describe fracture surfaces for three commercially available amorphous polymers (PC, PMMA and ABS) each subjected to tension, impact and environmental stress cracking (ESC). We present mechanical properties as well as microscopic characterization at low and high magnification to distinguish between slow tensile loading, fast impact loading, and enviro...

متن کامل

Fabrication of Polymer Electronic Boards by Ultrasonic Embossing and Welding

A method has been developed allowing fabrication of electronic boards from flexible polymer film by ultrasonic embossing and welding within seconds. A commercially available ultrasonic welding machine and micro patterned tools from aluminum are employed first to generate conductor paths on a flexible polymer film, in a further step, surface mounted devices (SMDs) are assembled and fixed on the ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Kobunshi

سال: 1993

ISSN: 0454-1138,2185-9825

DOI: 10.1295/kobunshi.42.403