Characteristics of Reheat Cracking in Weld Metal. Study of Reheat Cracking in FCAW Stainless Steel Weld Metal. (Report 1).
نویسندگان
چکیده
منابع مشابه
Crystallography of Widmanstätten austenite in duplex stainless steel weld metal
Two kinds of austenite grow from d-ferrite during the cooling of the duplex stainless steel weld deposits studied here, Widmanstätten plates and allotriomorphs which precipitate at d–d grain boundaries. It is found using microtexture measurements that the preferred crystallographic orientation of the Widmanstätten austenite can be estimated using established theory if it is assumed that there i...
متن کاملStainless steel weld metal designed to mitigate residual stresses
There have been considerable efforts to create welding consumables which on solid state phase transformation partly compensate for the stresses which develop when a constrained weld cools to ambient temperatures. All of these efforts have focused on structural steels which are ferritic. In the present work, alloy design methods have been used to create a stainless steel welding consumable which...
متن کاملAutomatic Segmentation of the Secondary Austenite-phase Island Precipitates in a Superduplex Stainless Steel Weld Metal
Victor H. C. Albuquerque & Rodrigo Y. M. Nakamura & João P. Papa Cleiton C. Silva & João Manuel R. S. Tavares Universidade de Fortaleza, Centro de Ciências Tecnológicas, Fortaleza, Brazil Departamento de Computação, UNESP Univ Estadual Paulista, Bauru, Brazil Departamento de Engenharia Metalúrgica e Materiais, Universidade Federal do Ceará, Fortaleza, Brazil Universidade do Porto, Faculdade de ...
متن کاملAn evaluation of weld metal nitrogen retention and properties in 316LN austenitic stainless steel
A series of tests were conducted using varying levels of nitrogen and helium in a conventional argon shielding gas when welding 316LN austenitic stainless steel. The outcome was that a 15 per cent nitrogen addition to the argon shielding gas had the most significant effect on increasing the weld metal nitrogen. Subsequent additions of helium to the argon 15 per cent nitrogen shielding gas had v...
متن کاملStress Corrosion Cracking Susceptibility of 304L Substrate and 308L Weld Metal Exposed to a Salt Spray
304 stainless steels (SS) were considered as the materials for a dry storage canister. In this study, ER (Electrode Rod) 308L was utilized as the filler metal for the groove and overlay welds of a 304L stainless steel substrate, which was prepared via a gas tungsten arc-welding process in multiple passes. The electron backscatter diffraction (EBSD) map was used to identify the inherent microstr...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY
سال: 2000
ISSN: 0288-4771
DOI: 10.2207/qjjws.18.59