Recovery of Copper from Copper Slag and Copper Slag Flotation Tailings by Oxidative Leaching

Copper smelter slag and copper smelter slag flotation tailings were leached using sulphuric acid solutions, without or with the addition of either ferric sulphate or hydrogen peroxide. Copper extraction from the slag was typically found to be twice as high as that from the slag flotation tailings. Hydrogen peroxide was determined to be the best lixiviant. Thus, copper and iron extractions were ...

متن کامل

Copper recovery from thickener overflow by electrocoagulation/flotation: optimization of response surface, modeling, and sludge study

The electrocoagulation/flotation process is a novel approach in mining industry that is implemented to return Cu metal to the production cycle, which improves copper recovery and reduces waste water. In this research work, the response surface methodology was applied to optimize the factors effective in Cu metal recovery and sludge volume produced from thickener overflow. To this end, the D-opt...

متن کامل

Effect of grinding time on flotation recovery of copper smelting slags in Bardaskan district

Copper smelting slags are hard materials. Therefore,to recover their copper by flotation method, grinding should be carried out to obtain optimal particle size. Copper smelting slags in the Bardeskan district, with work index of 16.24 kwh/st, were grinded for 65 minutes to reach an acceptable degree of freedom for the flotation tests, with particle size of 80%, smaller than 70 μm. With this gri...

متن کامل

Thermodynamic Investigation of Copper Removal From Liquid Slag.

The removal of copper dissolved in liquid stags by pyrometalIurgical means such as gaseous reduction and sulfidization is thermodynamically investigated. The lowest level possible for copper content is theoretically determined and compared. The results show that gaseous reduction is not as effective as sulfidization. Slags with very low levels of dissolved copper can be obtained with sulfide tr...

متن کامل

Vitrification of copper flotation waste.

The vitrification of an hazardous iron-rich waste (W), arising from slag flotation of copper production, was studied. Two glasses, containing 30wt% W were melted for 30min at 1400 degrees C. The first batch, labeled WSZ, was obtained by mixing W, blast furnace slag (S) and zeolite tuff (Z), whereas the second, labeled WG, was prepared by mixing W, glass cullet (G), sand and limestone. The glass...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Korean Institute of Resources Recycling

سال: 2015

ISSN: 1225-8326

DOI: 10.7844/kirr.2015.24.4.12