CFD Modeling of Macro-segregation and Shrinkage During Solidification of Superalloy Castings
نویسندگان
چکیده
منابع مشابه
Near-congruent solidification of castings
Chaput Kevin J. Ph.D., Purdue University, May 2015. Near-Congruent Solidification of Castings. Major Professor: Kevin Trumble. A study on the microstructure development of as-cast Cu-Mn alloys based around the congruent minimum at 34.6 wt % Mn and 873 oC was performed. Initially, this was to evaluate the alloy as an alternative to wide freezing range Pb and Sn bronzes that are plagued with poro...
متن کاملNumerical and Experimental Investigation of Solidification Shrinkage
The solidification heat transfer, melt convection and volume shrinkage in the casting of an energetic material are analyzed through numerical modeling and experimental investigation. The shrinkage resulting from phase change is considered through the volume of fluid method. The model is validated against an analytical solution and then applied to study the volume contraction during the casting ...
متن کاملChannel segregation during columnar solidification : influence of inertia
The numerical prediction of channel segregations during two-dimensional columnar solidification of Sn-Pb alloy is analyzed when inertia is considered in the dendritic mushy zone. This contribution is included in the momentum transport equation through the quadratic Forchheimer correction term. A significant influence of the Forchheimer term in the vicinity of the liquidus region is found. The n...
متن کاملeffectiveness of hedstroum files and rotary k3 instruments in removal of obturation materials during retreatment in curved canals
چکیده ندارد.
15 صفحه اولsimulation and experimental studies for prediction mineral scale formation in oil field during mixing of injection and formation water
abstract: mineral scaling in oil and gas production equipment is one of the most important problem that occurs while water injection and it has been recognized to be a major operational problem. the incompatibility between injected and formation waters may result in inorganic scale precipitation in the equipment and reservoir and then reduction of oil production rate and water injection rate. ...
ذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: ISIJ International
سال: 2010
ISSN: 0915-1559,1347-5460
DOI: 10.2355/isijinternational.50.1829