Cement Mortar Porosity by Modified Analysis of Differential Scanning Calorimetry Records

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Differential scanning calorimetry of bacteria.

Thermograms obtained by differential scanning calorimetry of a range of bacteria of different heat resistances were compared. Equations were derived to calculate the rate at which the numbers of viable organisms in a calorimeter decline as the temperature is raised at a constant rate. Vegetative bacteria scanned at 10 degrees C min-1 showed multi-peaked thermograms with four major peaks (denote...

متن کامل

Differential Scanning Calorimetry of Whole

Cereal Chem. 66(4):317-320 The thermal properties of whole grain milled rice and milled rice flour samples. Gelatinization enthalpies were about 40% greater in whole grain were investigated by differential scanning calorimetry. Thermal curves rice compared to rice flour for each variety. Heating rate studies conducted were obtained on representative long, medium, short, and very low amylose on ...

متن کامل

Differential scanning calorimetry of cytoplasmic aspartate transaminase.

Differential scanning calorimetry has been applied to study factors affecting the thermally induced denaturation of cytoplasmic aspartate aminotransferase, a dimeric pyridoxal enzyme. The consequences of binding of coenzyme and substrate derivatives to both the apo and holo forms of the enzyme were investigated and are interpreted in terms of the stabilization of the native form of the enzyme. ...

متن کامل

Study of rabies virus by Differential Scanning Calorimetry

Differential Scanning Calorimetry (DSC) has been used in the past to study the thermal unfolding of many different viruses. Here we present the first DSC analysis of rabies virus. We show that non-inactivated, purified rabies virus unfolds cooperatively in two events centered at approximately 62 and 73 °C. Beta-propiolactone (BPL) treatment does not alter significantly viral unfolding behavior,...

متن کامل

Measurement of Heat Capacity by Differential Scanning Calorimetry

The methods of measuring the heat capacity of materials by differential scanning calorimetry (DSC) are presented and discussed. The principles of temperature modulated DSC are outlined and the possibilities and limits of the method are discussed.

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials

سال: 2020

ISSN: 1996-1944

DOI: 10.3390/ma13051080