Development of Nondestructive Evaluation Methods for Ceramic Coatings and Membranes
Nondestructive evaluation (NDE) methods are being developed for thermal barrier coatings (TBCs) and for gas-separation membranes. For TBC applications, current NDE development is focused on infrared thermal imaging methods. Compared with optical and other methods, thermal imaging is quantitative so can be used to characterize TBCs during their entire life cycle, from as-processed condition to s...
متن کاملEffect of Porosity on Cavitation Erosion Resistance of HVOF Processed Tungsten Carbide Coatings
The phenomenon of cavitation is widely experienced in both pumps and under-water components of hydro power plants. The mechanism of material damage during cavitation is mainly attributed to implosion of high velocity bubbles on to the surface giving raise to local increase in stresses in excess of 1.4 GPa. In addition, material wastage due to particle induced erosion is observed in hydro plants...
متن کاملthe effect of functional/notional approach on the proficiency level of efl learners and its evaluation through functional test
in fact, this study focused on the following questions: 1. is there any difference between the effect of functional/notional approach and the structural approaches to language teaching on the proficiency test of efl learners? 2. can a rather innovative language test referred to as "functional test" ge devised so so to measure the proficiency test of efl learners, and thus be as much reliable an...
15 صفحه اولDevelopment of Nondestructive Evaluation Methods for Ceramic Coatings
Nondestructive evaluation (NDE) methods are being developed for ceramic thermal barrier coatings (TBCs) applied to components in the hot-gas path of advanced high-efficiency and low-emission gas turbines, including syn-gas fired turbines. The objectives of the NDE development are to assess TBC condition for quality control as well as to monitor TBC degradation and predict TBC life during servic...
متن کاملComparison of cavitation erosion rate with liquid impingement erosion rate
Both cavitation erosion and liquid impingement erosion are phenomena that can cause pipe wall thinning in power plants. The Code for Power Generation Facilities, Rules on Pipe Wall Thinning Management, was published by the JSME (Japan Society of Mechanical Engineers) in 2005. The code says that cavitation erosion shall be prevented either in the design stage or by daily inspection. On the other...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Zairyo-to-Kankyo
سال: 1995
ISSN: 0917-0480,1881-9664
DOI: 10.3323/jcorr1991.44.17