Boundary element analysis of galvanic corrosion problems - Computational accuracy on the galvanic field with screen plate.
نویسندگان
چکیده
منابع مشابه
Galvanic Corrosion Behavior of Dental Alloys
There is a wide variety of dental alloys, ranging from nearly pure gold and conventional gold-based alloys to alloys based on silver, palladium, nickel, cobalt, iron, titanium, tin, and other metals (Table 1). The types of dental alloys have increased significantly since 1980s in order to change the market price of gold and palladium. Although gold alloys are the mate‐ rials of choice in this a...
متن کاملComputational Simulation of Galvanic Corrosion under the Thin Film of Electrolyte
corrodes. The metal with the higher OCP acts as a cathode. On the cathode, reduction takes place. In the case of galvanic corrosion it is termed as depolarization. Electrolyte enables transport of the ions and the conductive connection closes an electric circuit. Electric current flowing between the electrode and the electrolyte causes a shift in the electrode potential. This phenomenon is call...
متن کاملAnalysis of the Temperature Influence on Galvanic Corrosion and Mathematical Model
The general and galvanic corrosion of high strength steel (980), high strength steel (907) and high strength steel (921A) in seawater at elevated temperatures has been analyzed using electrochemical measurements and a zero-resistance ammeter (ZRA). After the tests, the surface morphologies of the samples have been detected by SEM. Results show galvanic corrosion behavior of 980/907/921A fulfill...
متن کاملGalvanic corrosion between orthodontic wires and brackets in fluoride mouthwashes.
The aim of this investigation was to determine the influence of fluoride in certain mouthwashes on the risk of corrosion through galvanic coupling of orthodontic wires and brackets. Two titanium alloy wires, nickel-titanium (NiTi) and copper-nickel-titanium (CuNiTi), and the three most commonly used brackets, titanium (Ti), iron-chromium-nickel (FeCrNi) and cobalt-chromium (CoCr), were tested i...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 1989
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.38.1079