Atomic layer deposition of TiO2 thin films on glass fibers for enhanced photocatalytic activity
نویسندگان
چکیده
Photocatalytic wastewater treatment is expected to become a sustainable way of eliminating toxic chemicals. Due the surface-driven mechanism photocatalysis, surface area catalyst material plays crucial role in efficiency process, which usually achieved by nanoparticles. However, using powder materials introduces new problem: removing out clean water. As an alternative, atomic layer deposition (ALD) can form conformal thin films on high substrates providing immobilization route with photocatalytic activity. Textile are inexpensive and accessible therefore good candidates for substrate materials. Here, we deposit TiO2 fiberglass fabrics investigate Since as-deposited ALD amorphous, they have very limited Upon thermal after deposition, activity achieved. After four hours exposure solar simulator UV lamp, TiO2-coated fibers demonstrated much higher than planar previously described literature. The structure coated were investigated XRD, XPS, UV–Vis, PL analyses.
منابع مشابه
Atomic layer deposition of nano-TiO2 thin films with enhanced biocompatibility and antimicrobial activity for orthopedic implants
Titanium (Ti) and its alloys have been extensively used as implant materials in orthopedic applications. Nevertheless, implants may fail due to a lack of osseointegration and/or infection. The aim of this in vitro study was to endow an implant surface with favorable biological properties by the dual modification of surface chemistry and nanostructured topography. The application of a nanostruct...
متن کاملPhotocatalytic Degradation of Diazinon From Marine Source Using TiO2/SiO2 Thin Layer Coated on Glass
TiO2 photo catalyst was prepared in presence of nano SiO2 and Hydroxy Propyl Cellulose (HPC) by sol gel method with Titanium Tetra IsoproPoxide (TTIP) as titanium precursor. Additional effect of HPC in preparation of nano catalyst, and photo catalyst properties measured and characterized by FT-IR, FT-Raman and SEM. The catalyst size and structural properties of the film were determined by .-Ray...
متن کاملPhotocatalytic Properties of Co3O4-Coated TiO2 Powders Prepared by Plasma-Enhanced Atomic Layer Deposition
Co3O4-coated commercial TiO2 powders (P25) p-n junction photocatalysts were prepared by plasma-enhanced atomic layer deposition (PEALD) technique. The structure, morphology, bandgap, and photocatalytic properties under ultraviolet light were investigated systematically. Although the deposition of Co3O4 does not change the anatase structure and crystallite size of P25 powders, the ultraviolet ph...
متن کاملQuantum size effects in TiO2 thin films grown by atomic layer deposition
We study the atomic layer deposition of TiO2 by means of X-ray absorption spectroscopy. The Ti precursor, titanium isopropoxide, was used in combination with H2O on Si/SiO2 substrates that were heated at 200 °C. The low growth rate (0.15 Å/cycle) and the in situ characterization permitted to follow changes in the electronic structure of TiO2 in the sub-nanometer range, which are influenced by q...
متن کاملAtomic Layer Deposition of Noble Metal Thin Films
3 Preface 4 List of publications 5 List of symbols and abbreviations 6
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Materials Science: Materials in Electronics
سال: 2022
ISSN: ['1573-482X', '0957-4522']
DOI: https://doi.org/10.1007/s10854-022-08661-4