Atomic layer deposition of tin oxide and zinc tin oxide using tetraethyltin and ozone

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Incomplete elimination of precursor ligands during atomic layer deposition of zinc-oxide, tin-oxide, and zinc-tin-oxide.

For atomic layer deposition (ALD) of doped, ternary, and quaternary materials achieved by combining multiple binary ALD processes, it is often difficult to correlate the material properties and growth characteristics with the process parameters due to a limited understanding of the underlying surface chemistry. In this work, in situ Fourier transform infrared (FTIR) spectroscopy was employed du...

متن کامل

Atomic layer deposition of tin oxide films using tetrakis„dimethylamino... tin

The authors present a new method for preparing thin films of SnO2 by atomic layer deposition ALD using alternating exposures to tetrakis dimethylamino tin and hydrogen peroxide. This method avoids problems of corrosion and agglomeration associated with the halogenated compound, SnCl4. Tin oxide films were successfully deposited on a variety of substrates using deposition temperatures of 50–300 ...

متن کامل

Low Temperature Atomic Layer Deposition of Tin Oxide

Atomic layer deposition (ALD) of tin oxide (SnOx) films was achieved using a newly synthesized tin precursor and hydrogen peroxide. We obtained highly pure, conductive SnOx films at temperatures as low as 50 C, which was possible because of high chemical reactivity between the new Sn precursor and hydrogen peroxide. The growth per cycle is around 0.18 nm/cycle in the ALDwindow up to 150 C, and ...

متن کامل

Atomic Layer Deposition of Tin Oxide with Nitric Oxide as an Oxidant Gas

Atomic layer deposition (ALD) of tin oxide (SnO2) thin films was achieved using a cyclic amide of Sn(II) (1,3-bis(1,1-dimethylethyl)4,5-dimethyl-(4R,5R)-1,3,2-diazastannolidin-2-ylidene) as a tin precursor and nitric oxide (NO) as an oxidant gas. Film properties as a function of growth temperature from 130–250 C were studied. Highly conducting SnO2 films were obtained at 200–250 Cwith the growt...

متن کامل

Atomic layer deposited zinc tin oxide channel for amorphous oxide thin film transistors

Bottom-gate thin film transistors with amorphous zinc tin oxide channels were grown by atomic layer deposition. The films maintained their amorphous character up to temperatures over 500 C. The highest field effect mobility was 13 cm/V s with on-to-off ratios of drain current 10–10. The lowest subthreshold swing of 0.27 V/decade was observed with thermal oxide as a gate insulator. The channel l...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films

سال: 2015

ISSN: 0734-2101,1520-8559

DOI: 10.1116/1.4907562