Atomic layer deposition of photoelectrocatalytic material on 3D-printed nanocarbon structures
نویسندگان
چکیده
Combining two advanced layer-by-layer manufacturing techniques, low-temperature atomic layer deposition of MoS2 on a customizable 3D-printed nanocarbon surface, for photoelectrochemical energy conversion system.
منابع مشابه
Atomic layer deposition in porous structures: 3D photonic crystals
This paper reports recent results from studies of atomic layer deposition for the infiltration of three-dimensional photonic crystals. Infiltration of ZnS:Mn and TiO2 are reported for SiO2-based opal templates. It has been demonstrated that high filling fractions can be achieved and that the infiltrated material can be of high crystalline quality as assessed by photoluminescence measurements. T...
متن کاملMultiscale Simulation of Atomic Layer Deposition in a Nanoporous Material
A multiscale simulator for alumina film growth inside a nanoporous material during an atomic layer deposition process is developed. The model combines a continuum description at the macroscopic level of precursor gas transport inside a nanopore during exposure to each of the two precursor species (trimethyaluminum and water) with a lattice Monte Carlo simulation of the film growth on the micros...
متن کاملImpact of Atomic Layer Deposition to Nanophotonic Structures and Devices
*Correspondence: Muhammad Rizwan Saleem, Center for Energy Systems (CES), USAID Center for Advance Studies, National University of Sciences and Technology (NUST), Sector H-12, Islamabad 44000, Pakistan e-mail: [email protected]; [email protected] We review the significance of optical thin films by Atomic Layer Deposition (ALD) method to fabricate nanophotonic devices and structures. A...
متن کاملAtomic layer deposition (ALD): from precursors to thin film structures
The principles of the atomic layer deposition (ALD) method are presented emphasizing the importance of precursor and surface chemistry. With a proper adjustment of the experimental conditions, i.e. temperatures and pulsing times, the growth proceeds via saturative steps. Selected recent ALD processes developed for films used in microelectronics are described as examples. These include depositio...
متن کاملToward 3D Solid-State Batteries via Atomic Layer Deposition Approach
3D solid-state batteries are receiving great attentions as on-board power supply systems for small-dimension devices, due to their high power and energy densities. However, the fabrication of 3D solid-state batteries has been a formidable challenge due to the limitation of conventional thin-film techniques. Recently, atomic layer deposition (ALD) has emerged as a powerful approach toward 3D sol...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of materials chemistry. A, Materials for energy and sustainability
سال: 2021
ISSN: ['2050-7488', '2050-7496']
DOI: https://doi.org/10.1039/d1ta01467f