Atomic Layer Deposition of Lanthanum-Based Ternary Oxides
نویسندگان
چکیده
منابع مشابه
Atomic Layer Deposition of High-k Oxides on Graphene
Graphene that is a single hexagonal layer of carbon atoms with very high intrinsic charge carrier mobility (more than 200 000 cm2/Vs at 4.2 K for suspended samples; Bolotin, et al., 2008) attracts attention as a promising material for future nanoelectronics. During last few years, significant advancement has been made in preparation of large-area graphene. The lateral sizes of substrates for gr...
متن کاملAtomic Layer Deposition of TiO
Additional resources and features associated with this article are available within the HTML version: • Supporting Information • Links to the 4 articles that cite this article, as of the time of this article download • Access to high resolution figures • Links to articles and content related to this article • Copyright permission to reproduce figures and/or text from this article High surface a...
متن کاملParameter Space of Atomic Layer Deposition of Ultrathin Oxides on Graphene
Atomic layer deposition (ALD) of ultrathin aluminum oxide (AlOx) films was systematically studied on supported chemical vapor deposition (CVD) graphene. We show that by extending the precursor residence time, using either a multiple-pulse sequence or a soaking period, ultrathin continuous AlOx films can be achieved directly on graphene using standard H2O and trimethylaluminum (TMA) precursors e...
متن کاملGraphene oxide monolayers as atomically thin seeding layers for atomic layer deposition of metal oxides.
Graphene oxide (GO) was explored as an atomically-thin transferable seed layer for the atomic layer deposition (ALD) of dielectric materials on any substrate of choice. This approach does not require specific chemical groups on the target surface to initiate ALD. This establishes GO as a unique interface which enables the growth of dielectric materials on a wide range of substrate materials and...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Electrochemical and Solid-State Letters
سال: 2009
ISSN: 1099-0062
DOI: 10.1149/1.3074314