Atomic Layer Deposition of Copper Oxide using Copper(II) Acetylacetonate and Ozone
نویسندگان
چکیده
منابع مشابه
Atomic Layer Deposition of Fe2O3 Using Ferrocene and Ozone
Growing interest in Fe2O3 as a light harvesting layer in solar energy conversion devices stems from its unique combination of stability, nontoxicity, and exceptionally low material cost. Unfortunately, the known methods for conformally coating high aspect ratio structures with Fe2O3 leave a glaring gap in the technologically relevant temperature range of 170-350 C. Here, we elucidate a self-lim...
متن کاملAtomic Layer Deposition of Aluminum Oxide
I Acknowledgements II Dedication III List of Figures V
متن کاملSurface and interface processes during atomic layer deposition of copper on silicon oxide.
The initial surface chemistry and growth mechanisms of the atomic layer deposition (ALD) of metallic copper on SiO(2) surfaces are investigated using an amidinate precursor (copper(I) di-sec-butylacetamidinate, [Cu((s)Bu-amd)](2)) and molecular hydrogen. Using in situ Fourier transform infrared spectroscopy together with calculations based on density functional theory, we show that the initial ...
متن کاملAtomic Layer Deposition of a High-k Dielectric on MoS2 Using Trimethylaluminum and Ozone
We present an Al2O3 dielectric layer on molybdenum disulfide (MoS2), deposited using atomic layer deposition (ALD) with ozone/trimethylaluminum (TMA) and water/TMA as precursors. The results of atomic force microscopy and low-energy ion scattering spectroscopy show that using TMA and ozone as precursors leads to the formation of uniform Al2O3 layers, in contrast to the incomplete coverage we ob...
متن کاملLow Temperature Atomic Layer Deposition of Tin Oxide
Atomic layer deposition (ALD) of tin oxide (SnOx) films was achieved using a newly synthesized tin precursor and hydrogen peroxide. We obtained highly pure, conductive SnOx films at temperatures as low as 50 C, which was possible because of high chemical reactivity between the new Sn precursor and hydrogen peroxide. The growth per cycle is around 0.18 nm/cycle in the ALDwindow up to 150 C, and ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Chemical Vapor Deposition
سال: 2012
ISSN: 0948-1907
DOI: 10.1002/cvde.201106959