Graphene is a material with great promise for several applications within electronics. However, using graphene in any such application requires its integration stack of thin layers materials. The ideal structure has fully saturated surface without binding sites chemisorption growth species, making film on highly challenging. Herein, an attempt to deposit very AlN atomic layer deposition approach reported. It demonstrated X-ray photoelectron spectroscopy that Al–N are formed the films deposited and shown by scanning electron microscopy force have island morphology. These results may be considered promising toward development protocol possibly also 2D fabrication.
منابع مشابه
Atomic Layer Deposition of High-k Oxides on Graphene
Graphene that is a single hexagonal layer of carbon atoms with very high intrinsic charge carrier mobility (more than 200 000 cm2/Vs at 4.2 K for suspended samples; Bolotin, et al., 2008) attracts attention as a promising material for future nanoelectronics. During last few years, significant advancement has been made in preparation of large-area graphene. The lateral sizes of substrates for gr...
متن کاملUltrathin oxide films by atomic layer deposition on graphene.
In this paper, a method is presented to create and characterize mechanically robust, free-standing, ultrathin, oxide films with controlled, nanometer-scale thickness using atomic layer deposition (ALD) on graphene. Aluminum oxide films were deposited onto suspended graphene membranes using ALD. Subsequent etching of the graphene left pure aluminum oxide films only a few atoms in thickness. A pr...
متن کاملEpitaxial graphene surface preparation for atomic layer deposition of Al2O3
Atomic layer deposition was employed to deposit relatively thick ( 30 nm) aluminum oxide (Al2O3) using trimethylaluminum and triply-distilled H2O precursors onto epitaxial graphene grown on the Si-face of silicon carbide. Ex situ surface conditioning by a simple wet chemistry treatment was used to render the otherwise chemically inert graphene surface more amenable to dielectric deposition. The...
متن کاملDamage evaluation in graphene underlying atomic layer deposition dielectrics
Based on micro-Raman spectroscopy (μRS) and X-ray photoelectron spectroscopy (XPS), we study the structural damage incurred in monolayer (1L) and few-layer (FL) graphene subjected to atomic-layer deposition of HfO2 and Al2O3 upon different oxygen plasma power levels. We evaluate the damage level and the influence of the HfO2 thickness on graphene. The results indicate that in the case of Al2O3/...
متن کاملAtomic Layer Deposition of Titanium Oxide on Single-Layer Graphene: An Atomic-Scale Study toward Understanding Nucleation and Growth
Controlled synthesis of a hybrid nanomaterial based on titanium oxide and single-layer graphene (SLG) using atomic layer deposition (ALD) is reported here. The morphology and crystallinity of the oxide layer on SLG can be tuned mainly with the deposition temperature, achieving either a uniform amorphous layer at 60 °C or ∼2 nm individual nanocrystals on the SLG at 200 °C after only 20 ALD cycle...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Physica Status Solidi A-applications and Materials Science
سال: 2021
ISSN: ['1862-6300', '1862-6319']
DOI: https://doi.org/10.1002/pssa.202000684