Area-Selective Deposition of Ruthenium by Combining Atomic Layer Deposition and Selective Etching
نویسندگان
چکیده
منابع مشابه
Area-Selective Atomic Layer Deposition of Metal Oxides on Noble Metals through Catalytic Oxygen Activation
Area-selective atomic layer deposition (ALD) is envisioned to play a key role in next-generation semiconductor processing and can also provide new opportunities in the field of catalysis. In this work, we developed an approach for the area-selective deposition of metal oxides on noble metals. Using O2 gas as co-reactant, area-selective ALD has been achieved by relying on the catalytic dissociat...
متن کاملControlled Synthesis of Pd/Pt Core Shell Nanoparticles Using Area-selective Atomic Layer Deposition
We report an atomic scale controllable synthesis of Pd/Pt core shell nanoparticles (NPs) via area-selective atomic layer deposition (ALD) on a modified surface. The method involves utilizing octadecyltrichlorosilane (ODTS) self-assembled monolayers (SAMs) to modify the surface. Take the usage of pinholes on SAMs as active sites for the initial core nucleation, and subsequent selective depositio...
متن کاملBlocking the lateral film growth at the nanoscale in area-selective atomic layer deposition.
Area-selective atomic layer deposition (ALD) allows the growth of highly uniform thin inorganic films on certain parts of the substrate while preventing the film growth on other parts. Although the selective ALD growth is working well at the micron and submicron scale, it has failed at the nanoscale, especially near the interface where there is growth on one side and no-growth on the other side...
متن کاملSelective atomic layer deposition of titanium oxide on patterned self-assembled monolayers formed by microcontact printing.
We demonstrate a selective atomic layer deposition of TiO2 thin films on patterned alkylsiloxane self-assembled monolayers. Microcontact printing was done to prepare patterned monolayers of the alkylsiloxane on Si substrates. The patterned monolayers define and direct the selective deposition of the TiO2 thin film using atomic layer deposition. The selective atomic layer deposition is based on ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Chemistry of Materials
سال: 2019
ISSN: 0897-4756,1520-5002
DOI: 10.1021/acs.chemmater.9b00193