Applications and Advantages of Atomic Layer Deposition for Lithium-Ion Batteries Cathodes: Review

نویسندگان

چکیده

Nowadays, lithium-ion batteries (LIBs) are one of the most convenient, reliable, and promising power sources for portable electronics, tools, hybrid electric vehicles. The characteristics positive electrode (cathode active material, CAM) significantly contribute to battery’s functional properties. Applying various coatings is productive ways improve work batteries. there many methods depositing thin films on a material’s surface; among them, atomic layer deposition (ALD). ALD allows formation uniform surfaces with complex geometric forms, including porous structures. This review devoted applying method in obtaining cathode materials includes an overview more than 100 publications. thoroughly investigated surface modifications lithium cobalt oxide (LCO), manganese spinel (LMO), nickel-cobalt-manganese oxides (NCM), lithium-nickel-manganese (LNMO), lithium-manganese rich (LMR) materials. studied processes aluminum (Al2O3), titanium dioxide (TiO2) zirconium (ZrO2) films. primary purposes such studies find synthesis parameters films, optimal coating thickness (e.g., ~1–2 nm Al2O3, ~1 ZrO2, <1 TiO2, etc.), reveal effect electrochemical summarizes conditions, investigation results deposited CAMs electrodes some effects observed due obtained by cathodes.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electrode Materials for Lithium Ion Batteries: A Review

Electrochemical energy storage systems are categorized into different types, according to their mechanisms, including capacitors, supercapacitors, batteries and fuel cells. All battery systems include some main components: anode, cathode, an aqueous/non-aqueous electrolyte and a membrane that separates anode and cathode while being permeable to ions. Being one of the key parts of any new electr...

متن کامل

Ultrathin surface modification by atomic layer deposition on high voltage cathode LiNi0.5Mn1.5O4 for lithium ion batteries

Atomic layer deposition (ALD) has been employed to modify the surface of high voltage cathode LiNi0.5Mn1.5O4 by coating ultrathin Al2O3 layer on the electrodes. The ultrathin layer of Al2O3 can suppress the undesirable reactions during cycling, while maintaining the electron and ion conductivity of the electrode. The ALD Al2O3 coated LiNi0.5Mn1.5O4 showed remarkable improvement over bare LiNi0....

متن کامل

Li2MnSiO4 Nanostructured Cathodes for Rechargeable Lithium-Ion Batteries

Rechargeable lithium-ion battery technology dominates the portable electronics market following the rapid growth in demand since the introduction of the first, commercial lithium-ion battery by Sony in 1990 [1]. Motivated by concerns for global warming and environmental degradation, researchers have focused on extending the use of rechargeable lithium-ion batteries to large-scale applications. ...

متن کامل

Doped LiFePO4 Cathodes for High Power Density Lithium Ion Batteries

Olivine LiFePO4 has received much attention recently as a promising storage compound for cathodes in lithium ion batteries. It has an energy density similar to that of LiCoO 2, the current industry standard for cathode materials in lithium ion batteries, but with a lower raw materials cost and an increased level of safety. An inherent limitation of LiFePO4 acknowledged by researchers studying t...

متن کامل

Modification of Ni-Rich FCG NMC and NCA Cathodes by Atomic Layer Deposition: Preventing Surface Phase Transitions for High-Voltage Lithium-Ion Batteries

The energy density of current lithium-ion batteries (LIBs) based on layered LiMO2 cathodes (M = Ni, Mn, Co: NMC; M = Ni, Co, Al: NCA) needs to be improved significantly in order to compete with internal combustion engines and allow for widespread implementation of electric vehicles (EVs). In this report, we show that atomic layer deposition (ALD) of titania (TiO2) and alumina (Al2O3) on Ni-rich...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Batteries

سال: 2022

ISSN: ['2313-0105']

DOI: https://doi.org/10.3390/batteries8100184