In dye-sensitized photoelectrosynthesis cells (DSPECs) for water splitting or reduction of CO2, the most important figures merit are cell efficiency and stability. Maximizing these values requires use complex surface structures to perform key chemical reactions. The latter require a high level integrated research with focus on formation stabilization molecular both photoanodes photocathodes. Surface kinetics play element in dictating DSPEC efficiencies their control demands systematic design controlled local structures. ALD has been remarkably useful this area. It used fabrication core/shell structures, such as SnO2/TiO2 photoanodes, which greatly enhance charge separation significantly enhanced compared traditional TiO2 electrodes. extended form overlayer inert oxides preformed that lead stabilized impact resulting can have stability be profound, leading highly significant enhancement reactivity implications long-term catalysis. role significant. provided low-temperature, bottom-up approach creation chromophore/catalyst assemblies an increasingly electrodes interfacial energy conversion. Atomic layer deposition (ALD) extensively modification semiconductor surfaces scientific industrial applications. employs labile organometallic precursors add layers solids vacuum subsequently activated by hydrolysis. recent applications, it preparation molecularly based solar (DSSCs) This review focuses applications DSPECs fuels modified surfaces. area, prepare modify surface-interfacial electron transfer, stabilize surface-bound chromophores catalysts, oxidation photocathodes H2 CO2 reduction.
منابع مشابه
Interface Engineering through Atomic Layer Deposition towards Highly Improved Performance of Dye-Sensitized Solar Cells
A composite photoanode comprising ultralong ZnO nanobelts and TiO2 nanoparticles was prepared and its performance in dye-sensitized solar cells (DSSCs) was optimized and compared to the photoanode consisting of conventional TiO2 nanoparticles. The ultralong ZnO nanobelts were synthesized in high yield by a facile solution approach at 90°C followed by annealing at 500°C. The effect of the ratio ...
متن کاملSurface Modification of SnO2 Photoelectrodes in Dye-Sensitized Solar Cells: Significant Improvements in Photovoltage via Al2O3 Atomic Layer Deposition
We report here the exploitation of ultrathin layers of Al2O3 deposited via atomic layer deposition (ALD) on SnO2 photoanodes used in dye-sensitized solar cells featuring the I3 /I couple as the redox electrolyte. We find that a single ALD cycle of Al2O3 increases the lifetimes of injected electrons by more than 2 orders of magnitude. The modified SnO2 photoanode yields nearly a 2-fold improveme...
متن کاملApplication of azo dye as sensitizer in dye-sensitized solar cells
An azo dye used as photosensitizers in Dye-sensitized solar cells DSSCs. Azo dyes economically superior to organometallic dyes because they are color variation and cheap. The spectrophotometric evaluation of an azo dye in solution and on a TiO2 substrate show that the dye form J-aggregation on the nanostructured TiO2 substrate. Oxidation potential measurements for used azo dyes ensured an energ...
متن کاملStabilizing chromophore binding on TiO2 for long-term stability of dye-sensitized solar cells using multicomponent atomic layer deposition.
Ambient humidity and high temperature are known to degrade dye-sensitized solar cells (DSSCs) via chromophore desorption. Recently, enhanced dye-attachment to TiO2 surfaces has been realized by coating molecularly functionalized surfaces with inorganic atomic layer deposition (ALD) coatings. Here, we apply this ALD approach to DSSCs and demonstrate that high energy conversion efficiencies can b...
متن کاملInfluence of TiO2 layer thickness as photoanode in Dye Sensitized Solar Cells
Dye-sensitized solar cells (DSSCs) are categorized as some of inexpensive thin-film solar cells. The basis and foundation of these cells is a semiconductor that consists of an electrolyte and a light-sensitive anode. Titanium dioxide (TiO2) is a semiconductor that plays the role of anode and is the main constituent of these cells. In this paper, we have addressed the functionality and performan...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Trends in chemistry
سال: 2021
ISSN: ['2589-5974', '2589-7209']
DOI: https://doi.org/10.1016/j.trechm.2020.11.002