Anisotropy of nickel-based superalloy K418 fabricated by selective laser melting

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was cau...

متن کامل

Research on High Layer Thickness Fabricated of 316L by Selective Laser Melting

Selective laser melting (SLM) is a potential additive manufacturing (AM) technology. However, the application of SLM was confined due to low efficiency. To improve efficiency, SLM fabrication with a high layer thickness and fine powder was systematically researched, and the void areas and hollow powders can be reduced by using fine powder. Single-track experiments were used to narrow down proce...

متن کامل

Microstructures and Properties of 17-4 PH Stainless Steel Fabricated by Selective Laser Melting

Precipitation-hardened (PH) stainless steels have been widely used as structural materials and related applications in marine environments, power plants (light-water and pressurized water reactors), and chemical industries because of their good mechanical properties and corrosion resistance at typical service temperatures below 300oC. 17-4 PH (A1S1630) stainless steel (15–17.5 Cr, 3–5 Ni, 3–5 C...

متن کامل

A Comparison of Biocompatibility of a Titanium Alloy Fabricated by Electron Beam Melting and Selective Laser Melting

Electron beam melting (EBM) and selective laser melting (SLM) are two advanced rapid prototyping manufacturing technologies capable of fabricating complex structures and geometric shapes from metallic materials using computer tomography (CT) and Computer-aided Design (CAD) data. Compared to traditional technologies used for metallic products, EBM and SLM alter the mechanical, physical and chemi...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Progress in Natural Science: Materials International

سال: 2018

ISSN: 1002-0071

DOI: 10.1016/j.pnsc.2018.07.001