Anisotropy in Multiaxial Creep of a Nickel-Base Single-Crystal Superalloy CMSX-2. 2nd Report, Discussion Based on 3D Finite-Element Analysis.
نویسندگان
چکیده
منابع مشابه
Joining of nickel-base superalloy single crystals
Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................
متن کاملCrystal plasticity and crack initiation in a single-crystal nickel-base superalloy Modelling, evaluation and applications
In this dissertation the work done in the projects KME-410/502 will be presented. The overall objective in these projects is to evaluate and develop tools for designing against fatigue in single-crystal nickel-base superalloys in gas turbines. Experiments have been done on single-crystal nickel-base superalloy specimens in order to investigate the mechanical and fatigue behaviour of the materia...
متن کاملModelling of Thermomechanical Fatigue Stress Relaxation in a Single-Crystal Nickel-Base Superalloy
متن کامل
Modelling of constitutive and fatigue behaviour of a single-crystal nickel-base superalloy
In this licentiate thesis the work done in the project KME410 will be presented. The overall objective of this project is to evaluate and develop tools for designing against fatigue in single-crystal nickel-base superalloys in gas turbines. Experiments have been done on single-crystal nickel-base superalloy specimens in order to investigate the mechanical behaviour of the material. The constitu...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A
سال: 1992
ISSN: 0387-5008,1884-8338
DOI: 10.1299/kikaia.58.2446