Analysis of hydrogen embrittlement in zinc electroplating

نویسندگان

چکیده

Electrodeposition is the method of plating metal into another by hydrolysis generally to protect against corrosion metal. In Zinc Electroplating, deposited on steel, where acts as a sacrificial element that enhances Steel’s life. The zinc electroplating methods are mostly affected process parameters such current, temperature, voltage, etc. Hydrogen absorbed in plated layer and later it causes cracking, which known hydrogen embrittlement. De Embrittlement removes Hydrogen. Various test used qualify part after de-embrittlement. One them, Silicon oil was detect earlier now we have paraffin for same, thus making cost-efficient.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Prevention of Hydrogen Embrittlement in Steels

The essential facts about the nature of the hydrogen embrittlement of steels have now been known for 140 years. It is diffusible hydrogen that is harmful to the toughness of iron. It follows, therefore, that the harmful influence of diffusible hydrogen can be mitigated by preventing its entry into steel or by rendering it immobile once it penetrates the material. This review deals with the meth...

متن کامل

analysis of power in the network society

اندیشمندان و صاحب نظران علوم اجتماعی بر این باورند که مرحله تازه ای در تاریخ جوامع بشری اغاز شده است. ویژگیهای این جامعه نو را می توان پدیده هایی از جمله اقتصاد اطلاعاتی جهانی ، هندسه متغیر شبکه ای، فرهنگ مجاز واقعی ، توسعه حیرت انگیز فناوری های دیجیتال، خدمات پیوسته و نیز فشردگی زمان و مکان برشمرد. از سوی دیگر قدرت به عنوان موضوع اصلی علم سیاست جایگاه مهمی در روابط انسانی دارد، قدرت و بازتولید...

15 صفحه اول

Hydrogen Embrittlement of High Strength Steel Electroplated with Zinc-cobalt Alloys

Slow strain rate tests were performed on quenched and tempered AISI 4340 steel to measure the extent of hydrogen embrittlement caused by electroplating with zinc-cobalt alloys. The effects of bath composition and pH were studied and compared with results for electrodeposited cadmium and zinc-10%nickel. It was found that Zinc-1%cobalt alloy coatings caused serious hydrogen embrittlement (EI 0.63...

متن کامل

Characteristics of Hydrogen Embrittlement, Stress Corrosion Cracking and Tempered Martensite Embrittlement in High-strength Steels

Characteristics of tempered martensite embrittlement (TME), hydrogen embrittlement (HE), and stress corrosion cracking (SCC) in high-strength steels are reviewed. Often, it is important to determine unambiguously by which of these mechanisms failure occurred, in order to suggest the right actions to prevent failure recurrence. To this aim, samples made of high-strength AISI 4340 alloy steel wer...

متن کامل

Hydrogen embrittlement of grain boundaries in nickel: an atomistic study

The chemomechanical degradation of metals by hydrogen is widely observed, but not clearly understood at the atomic scale. Here we report an atomistic study of hydrogen embrittlement of grain boundaries in nickel. All the possible interstitial hydrogen sites at a given grain boundary are identified by a powerful geometrical approach of division of grain boundary via polyhedral packing units of a...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Science and Research Archive

سال: 2023

ISSN: ['2582-8185']

DOI: https://doi.org/10.30574/ijsra.2023.9.1.0369