An Experimental Study on Low-Cycle Fatigue Crack Initiation Life Prediction of Powder Superalloy FGH96 Based on the Manson-Coffin and Damage Mechanics Methods

نویسندگان

چکیده

The applicability of both prediction methods for low-cycle fatigue life powder superalloy based on the Manson-Coffin equation and damage mechanics were addressed. Both models evaluated by experimental data FGH96 with non-destructive standard parts those inclusions. Due to characteristics high strength low plasticity FGH96, errors in calculating plastic strain amplitude deviate severely outcomes when using method. Meanwhile, introducing variable which characterizes material damage, evolution can be built fitting also applied specimens containing inclusion. It is indispensable accurately calculate characterization parameter through finite element analysis local stress concentration around model was verified test cycles different types sizes inclusions subsequently. Testing simulation work showed much better accuracies globally approach.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Side Effects of Shot Peening on Fatigue Crack Initiation Life

Shot peening beneficial effects on fatigue life of mechanical components are well known. However, there are some reports in the literature that indicate inappropriate shot peening parameters tend to reduce the fatigue life. It is therefore, the purpose of this study to find a logical quantitative justification for these observations. Using finite element method, a dynamic elastic-plastic simula...

متن کامل

a study on the effectiveness of task types (noticing-reformulation) on iranian low intermediate efl learners’ retention of collocations

چکیده پژوهش شبه تجربی حاضر به بررسی بکارگیری تمارین کلاسی که برانگیزنده آگاهی و توجه آگاهانه به همایندها بعنوان بخشی از یک دوره ی مکالمه زبان خارجی در یکی از آموزشگاه های زبان انگلیسی ایران است می پردازد.

Energy-Based Prediction of Low-Cycle Fatigue Life of CK45 Steel and SS316 Stainless Steel

In this paper, low cycle fatigue life of CK45 steel and SS316 stainless steel under strain-controlled loading are experimentally investigated. In addition, the impact of mean strain and strain amplitude on the fatigue life and cyclic behavior of the materials are studied. Furthermore, it is attempted to predict fatigue life using energy and SWT damage parameters. The experimental results demons...

متن کامل

study the effects of low level laser diode on no production and healing of diabetic and cortisone acetate and normal wounded sd rats

nitric oxide (no) is a small molecule synthesized by most of mammalian cells with diverse biological activities including vasodilatation, host defense and wound healing. impaired wound healing is a common occurrence among diabetics and patients receiving glucocorticoid therapy. on the other hand the application of laser in biomedical area have been increased. thus, the current studies were desi...

15 صفحه اول

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2021

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met11030489