Recovery of Copper from Copper Slag and Copper Slag Flotation Tailings by Oxidative Leaching

Copper smelter slag and copper smelter slag flotation tailings were leached using sulphuric acid solutions, without or with the addition of either ferric sulphate or hydrogen peroxide. Copper extraction from the slag was typically found to be twice as high as that from the slag flotation tailings. Hydrogen peroxide was determined to be the best lixiviant. Thus, copper and iron extractions were ...

متن کامل

Copper Leaching Behavior from Waste Printed Circuit Board in Ammoniacal Alkaline Solution

A novel energy-saving hydrometallurgical recovery process for copper from electronic scrap employing the Cu(I)-ammine complex has been presented on the basis of a thermodynamic consideration. In order to experimentally explore the feasibility of the leaching stage in this process, the copper leaching behavior from a printed circuit board (PCB) in ammoniacal alkaline solutions has been investiga...

متن کامل

Copper recovery from ammoniacal media using hollow fibre contactors

This work aims to study the recovery of copper from ammoniacal aqueous solutions using hydrophobic propylene membrane contactors. The hydroxyoxime LIX 84-I and the β-diketone LIX 54 (both from Cognis) were used as extractants. The results obtained showed that practically all the copper content was removed from the ammoniacal feed solutions. The recovery of copper reached nearly 100% in several ...

متن کامل

Thermodynamic Investigation of Copper Removal From Liquid Slag.

The removal of copper dissolved in liquid stags by pyrometalIurgical means such as gaseous reduction and sulfidization is thermodynamically investigated. The lowest level possible for copper content is theoretically determined and compared. The results show that gaseous reduction is not as effective as sulfidization. Slags with very low levels of dissolved copper can be obtained with sulfide tr...

متن کامل

Optimized Leaching Conditions for Selenium from Sar-Cheshmeh Copper Anode Slimes

The recovery process of selenium from Iranian Sar-Cheshmeh copper anode slimes employing hydrometallurgical methods has been investigated. The copper anode slimes are made up of those components of  the anodes, which are not soluble in the electrolyte. They contain varying quantities of precious metals like gold, silver, selenium and tellurium. They are being extracted as a by product in th...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2020

ISSN: 2075-4701

DOI: 10.3390/met10060712