Alloy Design for Fe-Ni-Co-Al-based Superelastic Alloys

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Ternary Ni-Fe-Co Alloys Nanowire Electrodeposition

Nanowire is a cylindrical nano-structure with nanometer dimensions. In this research, the studied nanowire was made from the magnetic triple Ni-Fe-Co alloy.&#10 We utilized ordered porous anodic aluminum oxide as a template for the nanowire deposition. The nanowire arrays were electrodeposited in the cylindrical pores of the oxide layer by AC potential in a simple sulfate bath. Then the relatio...

متن کامل

Ternary Ni-Fe-Co Alloys Nanowire Electrodeposition

Nanowire is a cylindrical nano-structure with nanometer dimensions. In this research, the studied nanowire was made from the magnetic triple Ni-Fe-Co alloy. We utilized ordered porous anodic aluminum oxide as a template for the nanowire deposition. The nanowire arrays were electrodeposited in the cylindrical pores of the oxide layer by AC potential in a simple sulfate bath. Then the relation ...

متن کامل

CALCULATION OF THERMODYNAMIC PROPERTIES OF Al-Fe, Al-Ni AND Ni-Fe ALLOYS USING FACTSAGE

Thermodynamic predicting analysis of three binary systems Al-Fe, Al-Ni and Ni-Fe are shown in this paper. Thermodynamic analysis involved calculation of activities, coefficient of activities, partial and integral values for enthalpies and Gibbs energies of mixing and excess energies at three different temperatures: 1873K, 1900K and 1973K, as well as calculated phase diagrams, for the investigat...

متن کامل

Dental casting of superelastic Ni-Ti alloy.

Rods of Ni-43.5wt% Ti alloy were prepared under various casting conditions. Specimens which were melted in a cordierite crucible and cast in a phosphate-bonded investment mold had less strength and elongation than those melted in a copper crucible and cast in a phosphate-bonded investment mold. All castings exhibited superelasticity at room temperature. The upper limit of recoverable strain was...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Today: Proceedings

سال: 2015

ISSN: 2214-7853

DOI: 10.1016/j.matpr.2015.07.333