Accurate measurement of thin film mechanical properties using nanoindentation
نویسندگان
چکیده
Abstract For decades, nanoindentation has been used for measuring mechanical properties of films with the widely assumption that if indentation depth does not exceed 10% film thickness, substrate influence is negligible. The rule was originally deduced much thicker metallic on steel substrates and involved only hardness measurement. Thus, boundaries usability thin elastic modulus may differ. Two known material systems Mo MoTa Si are examined numerical modeling to show limitations in moduli. An assessment as a function contact accurate film/substrate deformation confirms measurements. modulus, depths should be smaller. Results provide recommended testing protocol using nanoindentation. Graphical abstract
منابع مشابه
Numerical study on the measurement of thin film mechanical properties by means of nanoindentation
Nanoindentation is a technique commonly used for measuring thin film mechanical properties such as hardness and stiffness. In this study, we used the finite element method to investigate the effect of substrate and pileup on hardness and stiffness measurements of thin film systems. We define a substrate effect factor and construct a map that may be useful in the interpretation of indentation me...
متن کاملQuantum Mechanical Simulations of Nanoindentation of Al Thin Film
QCDFT is a multiscale modeling approach that can simulate multi-million atoms effectively via density functional theory (DFT). The method is based on the framework of quasicontinuum (QC) approach with DFT as its sole energetics formulation. The local QC energy is calculated by DFT with Cauchy-Born hypothesis and the nonlocal QC energy is determined by a self-consistent embedding approach, which...
متن کاملMechanical Properties Measurement of Nanowires Anisotropic Conductive Film by Nanoindentation Technique
As microelectronic packaging industry grows explosively, high I/O density interconnects and reliable packaging design are recognized as the main concern of the IC packaging industry. Hence, in this investigation, a novel type of anisotropic conductive film (ACF) composed of cobalt nanowires and polymer was developed and used in place of conventional solder bumps for ultra-fine pitch interconnec...
متن کاملMechanical Properties of Cu2O Thin Films by Nanoindentation
In this study, the structural and nanomechanical properties of Cu₂O thin films are investigated by X-ray diffraction (XRD), atomic force microscopy (AFM), scanning electron microscopy (SEM) and nanoindentation techniques. The Cu₂O thin films are deposited on the glass substrates with the various growth temperatures of 150, 250 and 350 °C by using radio frequency magnetron sputtering. The XRD re...
متن کاملMeasurement of mechanical and thermal properties of co-sputtered WSi thin film for MEMS applications
In this study, mechanical and thermal properties of the co-sputtered tungsten silicide (WSi) thin film were evaluated to consider the possibility of its use in MEMS applications. WSi film was prepared by cosputtering and basic micromachining processes, and its mechanical and thermal properties such as Young’s modulus, temperature coefficient of resistance (TCR), strain gauge factor, coefficient...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Materials Research
سال: 2022
ISSN: ['0884-1616', '1092-8928', '0884-2914', '1091-8876', '2044-5326']
DOI: https://doi.org/10.1557/s43578-022-00541-1