A micromechanical analysis of intergranular stress corrosion cracking of an irradiated austenitic stainless steel

نویسندگان

چکیده

Irradiation Assisted Stress Corrosion Cracking (IASCC) is a material degradation phenomenon affecting austenitic stainless steels used in nuclear Pressurized Water Reactors (PWR), leading to the initiation and propagation of intergranular cracks. Such belongs broader class InterGranular (IGSCC). A micromechanical analysis IGSCC an irradiated steel performed this study assess local cracking conditions. 304L proton sample tested PWR environment showing investigated. Serial sectioning, Electron BackScatter Diffraction (EBSD) two-step misalignment procedure are reconstruct 3D microstructure over extended volume, statistically criteria. methodology also developed compute Grain Boundary (GB) normal orientations based on EBSD measurements. The statistical shows that occurs preferentially for GB normals aligned with mechanical loading axis, but low values Luster-Morris slip transmission parameter. Micromechanical simulations reconstructed microstructure, FFT-based solver crystal plasticity constitutive equations modified account at grain boundaries finally performed. These rationalize correlation obtained experimentally into single stress-based criterion. actual strengths weaknesses such approach discussed.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Stress Corrosion Cracking of an Austenitic Stainless Steel in Nitrite-Containing Chloride Solutions

This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC) in a nitrite-containing chloride solution. Slow strain rate testing (SSRT) in 30 wt. % MgCl₂ solution established SCC susceptibility, as evidenced by post-SSRT fractography. Addition of nitrite to the chloride solution, which is reported to have inhibitive influence on corrosion of stainless ste...

متن کامل

A Continuum Damage Model for the Stress Corrosion Cracking of Austenitic Stainless Steel

In the present work, the mechanical behavior of stress corrosion cracking phenomenon is described. Such phenomenon presents strong complexity due to metallurgic and electrochemical aspects. A methodology for modeling both SSR (Slow Strain Rate) and CL (Constant Load) tests based upon thermodynamics of continuum solids and elastoplastic damage is proposed. In this macroscopic approach, besides t...

متن کامل

An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution

The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...

متن کامل

Corrosion resistance of austenitic stainless steel in sulphuric acid

The resistance and susceptibility of austenitic stainless steel, Type 304, exposed to strong tetraoxosulphate (VI) acids (2 and 5 M concentrations) contaminated with sodium chloride at ambient temperatures was investigated by gravimetric and metallographic/scanning electron microscopy surface characterization methods. Scanning electron microscope (SEM) was used to examine and characterize the t...

متن کامل

Effects of irradiation on intergranular stress corrosion cracking

Intergranular stress corrosion cracking &YSCC) is a pervasive and generic problem in current light water reactor and advanced reactor designs that can lead to widespread component failure. IASCC is believed to be due to either to changes in the grain boundary composition, the microstructure or the water chemistry and corrosion potential. Of greatest interest are the changes in composition and m...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Materialia

سال: 2021

ISSN: ['1873-2453', '1359-6454']

DOI: https://doi.org/10.1016/j.actamat.2020.116482