A fractographic analysis of delamination within multidirectional carbon/epoxy laminates

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Delamination Analysis of Carbon Fibre Reinforced Laminates: Evaluation of a Special Step Drill

Drilling of carbon fibre/epoxy laminates is usually carried out using standard drills. However, it is necessary to adapt the processes and/or tooling as the risk of delamination, or other damages, is high. These problems can affect mechanical properties of produced parts, therefore, lower reliability. Production of higher quality holes is a challenge to everyone related with composites industry...

متن کامل

Wave Propagation Analysis in Composite Laminates Containing a Delamination Using a Three-Dimensional Spectral Element Method

A three-dimensional spectral element method SEM was developed for analysis of Lamb wave propagation in composite laminates containing a delamination. SEM is more efficient in simulating wave propagation in structures than conventional finite element method FEM because of its unique diagonal form of the mass matrix. Three types of composite laminates, namely, unidirectional-ply laminates, cross-...

متن کامل

Mode II delamination toughness of z-pinned laminates

Mode II delamination toughness of z-pin reinforced composite laminates is investigated using finite element (FE) method. The z-pin pullout process is simulated by the deformation and breakage of non-linear springs. A critical shear stress criterion based on linear elastic fracture mechanics is used to simulate crack growth in an end-notched-flexure (ENF) beam made of z-pinned laminates. The mod...

متن کامل

Compressive Behavior of a Glass/Epoxy Composite Laminates with Single Delamination

The buckling and postbuckling behaviors of a composite beam with single delamination are investigated. A three-dimensional finite element model using the commercial code ANSYS is employed for this purpose. The finite elements analyses have been performed using a linear buckling model based on the solution of the eigenvalues problem, and a non-linear one based on an incremental-iterative method....

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Composites Science and Technology

سال: 1995

ISSN: 0266-3538

DOI: 10.1016/0266-3538(95)00099-2