A Comparison between CoNiCrAlY Bond Coat and Zirconia Plasma Sprayed Coatings on Creep Tests
نویسندگان
چکیده
منابع مشابه
Air Plasma Sprayed Bond Coat Oxidation Behavior and its Resistance to Isothermal and Thermal Shock Loading
An experimental investigation was conducted to find the effect of spraying method of coating of Thermal Barrier Coatings (TBCs) on their oxidation behaviour and resistance to various thermal loading. Isothermal and thermal shock tests were performed in order to study oxidation behaviour of air plasma sprayed Bond Coat (BC) and assess its effect on TBCs lifetime under the stated loadings. Specim...
متن کاملEffects of pores and interfaces on effective properties of plasma sprayed zirconia coatings
It is difficult to establish structure–property relationships in plasma sprayed coatings because of their unique and intermingled splat microstructures incorporating networks of various intrinsic process-dependent microdefects. In this paper, these coatings are characterized using two distinctly different approaches, both based on novel experimental techniques and computational modeling tools. ...
متن کاملNon-linear elastic properties of plasma-sprayed zirconia coatings and associated relationships with processing conditions
Low-temperature thermal cycling of plasma-sprayed zirconia coatings via curvature measurements revealed their in-plane non-linear behavior. This feature arises from the unique layered, porous and cracked morphology of thermal-sprayed ceramic materials. The nonlinear aspect can be quantified by a novel data interpretation procedure consisting of modified beam bending analysis and inverse analysi...
متن کاملBond Strength of Plasma Sprayed Ceramic Coatings on the Phosphated Steels
P. Pokorny, L. Mastny, V. Sykora, Institute of Chemical Technology Prague, Czech Republic Z. Pala, V. Brozek, Institute of Plasma Physics ASCR v.v.i. Prague, Czech Republic In the presented work, results of adhesion measurements for different systems of steel sheet-phosphate interlayerceramic coating are described. The interlayers were produced by zinc phosphating; alumina, olivine and zirconia...
متن کاملMicrostructure formation in plasma-sprayed functionally graded NiCoCrAlY/yttria-stabilized zirconia coatings
Functionally graded NiCoCrAlY/yttria-stabilized zirconia coatings were fabricated by plasma spraying using mechanically alloyed, plasma-spheroidized NiCoCrAlY/yttria-stabilized zirconia (YSZ) composite powders. Scanning electron microscopy (SEM) and energy dispersive X-ray spectrometry (EDS) analysis revealed that oxidation of aluminum, chromium and yttrium in the NiCoCrAlY alloy occurred in th...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science Forum
سال: 2008
ISSN: 1662-9752
DOI: 10.4028/www.scientific.net/msf.591-593.30