Effect of Mean Stress on Fatigue Crack Growth Behavior of Stainless Steel 304L

Stainless steel has been employed in many engineering applications ranging from pharmaceutical equipment to piping in the nuclear reactors and storage to chemical products. In this attempt, simulation of fatigue crack growth based on experimental results of austenitic stainless steel 304L was presented using AFGROW code when NASGRO mode laws adopted. Double through crack at hole specimen is use...

متن کامل

Relaxation Peaks of Cold Worked 304l Stainless Steel

In this investigation internal friction of cold worked 304L austenitic stainless steel was measured and the new peaks (PlIP2,P3) were found. The height of those peaks increased with cold work degree. The temperature of the main peak P3 was 33513340K at the frequency of -1,000Hz. The activation energies and frequency factors were obtained from peak shift. The values were 0.4evl 0.4evl 0.6ev and ...

متن کامل

Mechanical Evaluation of Stainless Steel and Titanium Dynamic Hip Screws for Trochanteric Fracture

This study aimed to present the mechanical performance evaluation of the dynamic hip screw (DHS) for trochanteric fracture by means of finite element method. The analyses were performed based on stainless steel and titanium implant material definitions at various stages of bone healing and including implant removal. The assessment of the mechanical performance used two parameters, von Mises str...

متن کامل

Welding of 304L Stainless Steel to 409 Stainless Steel with GMAW Process Using ER316LSi and ER309LMo Filler Metals

Dissimilar welding of AISI 304L austenitic stainless steel to AISI 409 ferritic stainless steel with GMAW process usingtwo Ar-O2 and Ar-CO2 shielding gas mixtures was studied. ER316LSi and ER309LMo filler metals were chosen by considering 5 and 15% delta ferrite according to the Schaeffler equations and diagram. Based on the observations, both filler metals accompanied by Ar-2%O2 shielding gas ...

متن کامل

Welding of 304L Stainless Steel to 409 Stainless Steel with GMAW Process Using ER316LSi and ER309LMo Filler Metals

Dissimilar welding of AISI 304L austenitic stainless steel to AISI 409 ferritic stainless steel with GMAW process usingtwo Ar-O2 and Ar-CO2 shielding gas mixtures was studied. ER316LSi and ER309LMo filler metals were chosen by considering 5 and 15% delta ferrite according to the Schaeffler equations and diagram. Based on the observations, both filler metals accompanied by Ar-2%O2 shielding gas ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Ubiquity Proceedings

سال: 2018

ISSN: 2631-5602

DOI: 10.5334/uproc.41